Nyenzo ya thermoplastiki ya alama inayowekwa kwa joto na kutengenezwa chini ya mfumo wa fomula wa BS 3262 — kiwango kinachotajwa sana katika zabuni zenye ushawishi wa Uingereza barani Afrika, Mashariki ya Kati na Asia ya Kusini-Mashariki. Inapatikana nyeupe na njano, ikirekebishwa kifungu kwa kifungu kulingana na zabuni yako, pamoja na karatasi ya data na sampuli za bure kabla hujaweka ahadi.
BS 3262 ni mkusanyiko wa sehemu tatu, mbili kati yake ziliondolewa mwaka 2000 — miradi ya kisasa kwa kawaida huunganisha mfumo wake wa fomula na vifungu vya utendaji vya EN, nasi tunatengeneza fomula kwa yote mawili. Majedwali yaliyo hapa chini yananukuu mahitaji ya maandishi asilia.
| Composition (% of total mixture) | Requirement |
|---|---|
| Binder (resin + oil) | 20 ± 2% |
| Premixed solid glass beads (when reflectorized) | ≥ 20% |
| Aggregate + pigment + filler + premix beads, combined | 80 ± 2% |
The premix beads sit inside the 80 ± 2% total. White pigment must be anatase or rutile titanium dioxide to BS 1851 — the standard fixes the type, not a minimum content. The combined solids must pass a 2.80 mm sieve completely, with 65–95% passing 600 µm.
| Property | White | Yellow |
|---|---|---|
| Softening point | ≥ 65°C | ≥ 65°C |
| Luminance factor, as manufactured | ≥ 70 | ≥ 50 |
| Luminance factor, remelted on site | ≥ 65 | ≥ 45 |
| Luminance factor after heat-stability test | ≥ 65 | ≥ 45 |
| Flow resistance (mean slump) | ≤ 25% | ≤ 25% |
| Laboratory skid resistance (pendulum) | ≥ 45 | ≥ 45 |
The heat-stability test stirs the material for six hours at 200°C or the declared maximum application temperature, whichever is lower. Luminance factor is a daytime whiteness figure — it is not the night-time retroreflectivity (RL) of EN 1436; if your tender sets an RL target, specify it separately and we formulate for it.
| Binder system | Method | Thickness (excl. drop-on beads) |
|---|---|---|
| Synthetic resin | Screed | 2.0 – 5.0 mm |
| Spray (except yellow edge lines) | ≥ 1.5 mm | |
| Extrusion | 2.5 – 3.5 mm | |
| Gum / wood rosin | Screed | 3.0 – 5.0 mm |
| Spray (except yellow edge lines) | ≥ 2.0 mm | |
| Extrusion | 4.0 – 5.0 mm |
Lay on a dry surface above 5°C; concrete and polished-aggregate asphalt need a compatible primer. Line width tolerance is +10% / −5% of the specified width.
Kile ambacho BS 3262 inahitaji hasa — na kile ambacho haihitaji
VIFUNGU SABA VINAVYOTUMIKA SANA KWENYE ZABUNI HAVIMO KWENYE MAANDISHI YA KIWANGO. WAHANDISI WETU WANACHAMBUA MAANDISHI ASILIA, JEDWALI KWA JEDWALI.


Yes — free samples of 1–2 kg for any product. Whatever you pay for the sample and its freight is credited in full against your next purchase. Email info@pztraffic.com with the products and standards you need.
Yes. Clauses like softening point ≥ 95°C, TiO₂ ≥ 10% or an initial RL figure are project add-ons, not part of the standard’s original text — so they must be stated explicitly. Send us the tender clause and we formulate against it, answering with a datasheet that covers every line.
Yes, both forms. Premix beads can be built into the material at the plant — our 20% mixed glass beads variant matches the standard’s reflectorized formulation — and drop-on beads (BS 6088B, AASHTO M247 types) ship alongside the paint in the same container.